Modification of a natural zeolite with Fe(III) for simultaneous phosphate and ammonium removal from aqueous solutions

BACKGROUND: The incorporation of Fe(III) was performed in a natural clinoptilolite (Z-N) for simultaneous phosphate and ammonium removal. RESULTS: The existence of hydroxyl groups (?Fe-OH) in the iron zeolite (Z-Fe) enhances the phosphate uptake from 0.6�0.1mg-P g-1 in Z-N to 3.4�0.2mg-P g-1 in Z-Fe...

Descrizione completa

Salvato in:
Dettagli Bibliografici
Autore principale: Guaya Caraguay, D. (author)
Altri autori: Farran, A. (author), Valderrama, C. (author), Cortina, J. (author)
Natura: article
Pubblicazione: 2016
Soggetti:
Accesso online:http://dspace.utpl.edu.ec/handle/123456789/19000
Tags: Aggiungi Tag
Nessun Tag, puoi essere il primo ad aggiungerne!!
Descrizione
Riassunto:BACKGROUND: The incorporation of Fe(III) was performed in a natural clinoptilolite (Z-N) for simultaneous phosphate and ammonium removal. RESULTS: The existence of hydroxyl groups (?Fe-OH) in the iron zeolite (Z-Fe) enhances the phosphate uptake from 0.6�0.1mg-P g-1 in Z-N to 3.4�0.2mg-P g-1 in Z-Fe. However, the ammonium sorption capacity slightly decreases from 33�2mg-Ng-1 in Z-N to 27�2mg-Ng-1 in Z-Fe. The equilibrium and kinetics sorption were well explained by the Langmuir isotherm and the intraparticle diffusion model, respectively. CONCLUSIONS: Both the phosphate and ammonium uptake were slightly affected by the coexistence of competing ions. The phosphate sorption capacity of iron zeolite was decreased in the regeneration cycles. Desorption using a 1molL-1 NaOH solution under dynamic conditions provided higher enrichment factors for ammonium than phosphate. © 2015 Society of Chemical Industry.